Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terblend® N NM-19 XP - (ABS+PA6) - INEOS Styrolution

Material Data Center offers the following functions for Terblend® N NM-19 XP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Terblend N datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Terblend® N NM-19 XP is an UV stabilised ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearance.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 40 / * cm³/10min ISO 1133
Temperature 240 / * °C -
Load 10 / * kg -
Molding shrinkage, parallel 0.7 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Density of melt 928 kg/m³ -
Thermal conductivity of melt 0.156 W/(m K) -
Spec. heat capacity of melt 2410 J/(kg K) -
Ejection temperature 90 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2000 / 1400 MPa ISO 527
Yield stress 43 / 34 MPa ISO 527
Yield strain 3.5 / 5.5 % ISO 527
Nominal strain at break 30 / 35 % ISO 527
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 65 / - kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 15 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 65 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 85 / * °C ISO 75-1/-2
Vicat softening temperature, B 102 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 100 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.3 / - - IEC 62631-2-1
Relative permittivity, 1MHz 2.9 / 3.3 - IEC 62631-2-1
Dissipation factor, 1MHz 150 / 550 E-4 IEC 62631-2-1
Volume resistivity >1E13 / 1E11 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E14 Ohm IEC 62631-3-2
Comparative tracking index 600 / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Humidity absorption 1.2 / * % Sim. to ISO 62
Density 1070 / - kg/m³ ISO 1183
Diagrams
Dynamic Shear modulus-temperature , Terblend® N NM-19 XP, (ABS+PA6), INEOS Styrolution
Stress-strain (isochronous) 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Creep modulus-time 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Creep curve 23°C, Terblend® N NM-19 XP (cond.), (ABS+PA6), INEOS Styrolution
Stress-strain (isochronous) 60°C, Terblend® N NM-19 XP (dry), (ABS+PA6), INEOS Styrolution
Creep modulus-time 60°C, Terblend® N NM-19 XP (dry), (ABS+PA6), INEOS Styrolution
Creep curve 60°C, Terblend® N NM-19 XP (dry), (ABS+PA6), INEOS Styrolution
Specific volume-temperature (pvT) , Terblend® N NM-19 XP, (ABS+PA6), INEOS Styrolution
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 240 - 270 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
Chemical Media Resistance
Acids
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.